The new merchant cargo ships use a large variety of steels in their construction; the steels range in yield strength from 40 to 100 ksi. Some of these steels require a close control of the welding procedure as well as other special techniques, to assure serviceability, and a special repair welding procedure must be developed, applicable for all strengths of steel used in construction and requiring a minimum amount of procedure control. The recommended temporary welding repair procedure and a discussion of the survey which led to the recommendation are described in this report. (Author).The new merchant cargo ships use a large variety of steels in their construction; the steels range in yield strength from 40 to 100 ksi.
Title | : | Recommended Emergency Welding Procedure for Temporary Repairs of Ship Steels |
Author | : | A. L. Lowenberg, P. D. Watson, SOUTHWEST RESEARCH INST SAN ANTONIO TEX. |
Publisher | : | - 1969 |
You must register with us as either a Registered User before you can Download this Book. You'll be greeted by a simple sign-up page.
Once you have finished the sign-up process, you will be redirected to your download Book page.
How it works: